Title: Fluoride-containing adhesive: Durability on dentin bonding
Author: Shinohara, MS
De Goes, MF
Schneider, LFJ
Ferracane, JL
Pereira, PNR
Di Hipolito, V
Nikaido, T
Abstract: Objectives. To evaluate (1) the influence of fluoride-containing adhesive on microtensile bond strength (mu TBS) and (2) in vitro secondary caries inhibition at the resin-dentin interface after 24h and 3 months water-storage and (3) the degree of conversion of different adhesives after 24h 1 month. Methods. Flat surfaces of human teeth were ground and randomly assigned to six groups: (SBMP-24) Scotchbond Multi-Purpose control [SBMP], 24 h; (SE-24) SBMP etch and primer + Clearfil SE Bond adhesive [SE], 24 h; (PB-24) SBMP etch and primer + Clearfil Protect Bond adhesive [PB], 24 h; (SBMP-3) SBMP, 3 months; (SE-3) SBMP+SE, 3 months; and (PB-3) SBMP+PB, 3 months. To evaluate the effect of the adhesive resin alone, all teeth were etched with 35% phosphoric acid and primed with SBMP primer prior to applying the adhesive resin. Bonded assemblies were prepared for mu TBS and stored in distilled water at 37 degrees C for 24h and 3 months. Sections of restored teeth of each group were exposed to an acid challenge. The specimens were sectioned, polished, and then observed with polarized light microscopy (PLM). Also, the degree of conversion (DC) of the adhesives was measured using Fourier Transform-Infrared spectroscopy (FTIR) at 24h and 1 month, after polymerization. Results. mu TBS values obtained in MPa (24 h/3 m) were: (MP) 61.5 +/- 10.5/52.9 +/- 8.9, (SE) 55.5 +/- 11.8/55.6 +/- 13, and (PB) 50.3 +/- 9.9/ 61.0 +/- 13.6. For interface analysis by PLM, an inhibition zone (IZ) adjacent to the hybrid layer was created only when the fluoride-containing adhesive (PB) was used. The DC in percentage (24 h, 1 month) were: (MP) 60.5 +/- 2.8/61.3 +/- 0.6, (SE) 69.6 +/- 1.3/70.7 +/- 0.05, and (PB) 53.1 +/- 0.4/58.3 +/- 1.6. Significance. The. uoride-containing adhesive demonstrated significant increase of bond strength values after water-storage. This material was also able to create an acid inhibition zone in dentin. There was a significant increase of degree of conversion after 1 month only for PB. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Subject: Adhesive system
Dentin
Durability
Fluoride-containing material
Hybrid layer
Inhibition zone
Microtensile bond strength
Outer lesion
Polarized light microscopy
Secondary caries
Country: Inglaterra
Editor: Elsevier Sci Ltd
Rights: fechado
Identifier DOI: 10.1016/j.dental.2009.06.011
Date Issue: 2009
Appears in Collections:Unicamp - Artigos e Outros Documentos

Files in This Item:
File Description SizeFormat 
WOS000271471600011.pdf996.69 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.