Please use this identifier to cite or link to this item: http://repositorio.unicamp.br/jspui/handle/REPOSIP/67241
Type: Artigo de periódico
Title: FTIR study of hydrogen and carbon monoxide adsorption on Pt/TiO2, Pt/ZrO2, and Pt/Al2O3
Author: Benvenutti, EV
Franken, L
Moro, CC
Davanzo, CU
Abstract: The Pt/TiO2, Pt/ZrO2, and Pt/Al2O3 catalysts submitted to low-temperature reduction (LTR, 200 degrees C) and high-temperature reduction (HTR, 500 degrees C) and exposed to hydrogen and carbon monoxide at room temperature were studied by infrared spectroscopy. There is a strong loss of transmission in the entire infrared spectra on Pt/TiO2 after its exposure to hydrogen, which is related to the reducibility of the support. A typical SMSI behavior (strong metal-support interaction), such as the decrease in carbon monoxide adsorption capacity, was detected on Pt/TiO2 and Pt/ZrO2 after exposure to hydrogen, even for the catalysts submitted to LTR treatment. Also a carbonyl band shift to lower wavenumber was observed on LTR-treated Pt/TiO2, Pt/ZrO2, and Pt/Al2O3 after exposure to hydrogen. We interpreted this SMSI behavior as an electronic rather than morphological effect, which was induced by the presence of hydrogen spillover.
Country: EUA
Editor: Amer Chemical Soc
Rights: fechado
Identifier DOI: 10.1021/la990195s
Date Issue: 1999
Appears in Collections:Artigos e Materiais de Revistas Científicas - Unicamp

Files in This Item:
File Description SizeFormat 
WOS000083684600038.pdf90.5 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.