Title: Effects of Reducing Agents on Birefringence Dentin Collagen after Use of Different Endodontic Auxiliary Chemical Substances
Author: Moreira, DM
Feitosa, JPD
Line, SRP
Zaia, AA
Abstract: Introduction: The aim of this study was to evaluate the effect of 10% ascorbic acid or 10% sodium ascorbate on organic matrix collagen of bovine dentin root canal walls after irrigation with 5.25% sodium hypochlorite (NaOCl), 17% ethylenediaminetetraacetic acid (EDTA), or 0.9% sodium chloride. Methods: Eighty bovine incisors were randomly divided into 8 groups (n = 10): group 1, 0.9% sodium chloride (control); group 2, 5.25% NaOCl + 17% EDTA (NaOCl + EDTA); group 3, 5.25% NaOCl + 17% EDTA + 10% ascorbic acid (NaOCl + EDTA + AA); group 4, 5.25% NaOCl + 17% EDTA + 10% sodium ascorbate (NaOCl + EDTA + SA); group 5, 5.25% NaOCl (NaOCl); group 6, 17% EDTA; group 7, 10% ascorbic acid (AA); and group 8, 10% sodium ascorbate (SA). Teeth were chemomechanically prepared, submitted to histologic processing, and stained with Sirius Red dye to be analyzed under polarized light microscopy. Absorbance assay was also performed to confirm the loss of collagen. Results: NaOCl + EDTA and NaOCl groups presented a significantly different birefringence pattern compared with the control group (P < .05). The measurement of the optical retardations of NaOCl + EDTA + SA indicated that this group was not statistically different from the control group. Although the measurement of the optical retardations of NaOCl + EDTA + AA was statistically different from the control group, the results were significantly higher than for NaOCl + EDTA. The birefringence of EDTA, AA, and SA groups was not statistically different from that of control group. The absorbance assay of NaOCl + EDTA and NaOCl groups confirmed the loss of collagen (P<.05). Conclusions: It is possible to conclude that 5.25% NaOCl, whether associated or not with 17% EDTA, causes birefringence alterations and loss of dentin collagen. These alterations reduced the ability of Sirius Red to bind with collagen fiber molecules. The reductions in the optical retardation values could be reversed by the application of either 10% ascorbic acid or 10% sodium ascorbate after 5.25% sodium hypochlorite and 17% EDTA irrigation. (J Endod 2011;37:1406-1411)
Subject: Auxiliary chemical solutions
birefringence
collagen
reducing agents
Country: EUA
Editor: Elsevier Science Inc
Rights: fechado
Identifier DOI: 10.1016/j.joen.2011.06.026
Date Issue: 2011
Appears in Collections:Unicamp - Artigos e Outros Documentos

Files in This Item:
File Description SizeFormat 
WOS000295661800015.pdf1.15 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.