Please use this identifier to cite or link to this item: http://repositorio.unicamp.br/jspui/handle/REPOSIP/263821
Full metadata record
DC FieldValueLanguage
dc.contributor.CRUESPUNIVERSIDADE ESTADUAL DE CAMPINASpt_BR
dc.identifier(Broch.)pt_BR
dc.descriptionOrientador: Eliana Aparecida de Rezende Duekpt_BR
dc.descriptionDissertação (mestrado) - Universidade Estadual de Campinas, Faculdade de Engenharia Mecanicapt_BR
dc.format.extent92p. : il.pt_BR
dc.format.mimetypeapplication/pdfpt_BR
dc.languagePortuguêspt_BR
dc.typeDISSERTAÇÃOpt_BR
dc.titleOsteointegração de blendas de PLDLA/PCL : estudo in vitro e in vivopt_BR
dc.title.alternativeOsteointegration of PLDLA/PCL blends : in vitro and in vivo studypt_BR
dc.contributor.authorPinto, Marcelo Robertopt_BR
dc.contributor.advisorDuek, Eliana Aparecida de Rezende, 1961-pt_BR
dc.contributor.institutionUniversidade Estadual de Campinas. Faculdade de Engenharia Mecânicapt_BR
dc.contributor.nameofprogramPrograma de Pós-Graduação em Engenharia Mecânicapt_BR
dc.subjectHistologiapt_BR
dc.subjectPolímeros na medicinapt_BR
dc.subject.otherlanguageHistologyen
dc.subject.otherlanguagePolymers in medicineen
dc.description.abstractResumo: Os polímeros bioreabsorvíveis apresentam grande potencial de uso biomédico, pois são geralmente, fáceis de processar e apresentam características mecânicas semelhantes aos dos materiais biológicos, como é o caso do poli(L-ácido lático) amplamente estudado nas últimas décadas. Uma maneira de modificar as propriedades de um homopolímero para aplicações ortopédicas é a obtenção de blendas, visando melhorar suas propriedades comparando-se aos polímeros puros. Contudo, esse trabalho tem por objetivo: 1 ) avaliar a degradação in vitro das blendas de PLDLA/PCL, nas proporções 100/0, 90/10, 80/20 e 70/30 e caracterizá-las através de análises de MEV, DSC, GPC e ensaio mecânico antes e após degradação das amostras em tampão fosfato. 2) realizar o estudo in vivo. Os resultados in vitro, revelaram que até o período de 180 dias, todos os materiais estudados (PLDLA/PCL) nas composições 100/0, 90/10, 80/20 e 70/30, a partir das análises de DSC, MEV e ensaio mecânico apresentaram discretos sinais de degradação, e após o período de 180 dias todos os materiais apresentavam se degradados. Das análises realizadas, o GPC foi a mais sensível, ou seja, embora se verifique perda de massa molar, as propriedades térmicas são estáveis, o mesmo pode ser obervados nas análises de DSC. As propriedades mecânicas das blendas não apresentaram alterações significativas até 180 dias de degradação, revelando que a blenda torna-se mais elástica e menos frágil com a adição de PCL. As análises de MEV reveleram uma discreta degradação da blenda 70/30 em 180 dias e completa degradação de todas as amostras após 220 dias. A partir do estudo in vitro, escolheu-se as blendas (PLDLA/PCL) 100/0 e 70/30 para o estudo in vivo. Os resultados revelaram que o grau de organização tecidual se estabeleceu em função do período de implante. Até o período de 180 dias não houve diferença in vivo relevante entre os pinos de PLDLA puro e da blenda PLDLA/PCL (70/30). Nesse experimento os cortes histológicos revelaram ausência de células inflamatórias e reações de corpo estranho na interface óssea em períodos mais longos de implantes. Foi predominante a presença de células ósteo-progenitoras povoando a interface por tecido mineralizado ao redor dos polímerospt
dc.description.abstractAbstract: Bioreabsorbable polymers present great potential in biomedical applications, because they are usually, easy to process and they present a similar biological mechanical characteristics, as it is the case of poly(L- lactic acid) very studied in the last decades. A way to modify the properties of a homopolymer for orthopedic applications is obtention of blends, aiming to improve their properties compared to the pure polymers. The aim of this study was: 1) to evaluate the in vitro degradation of PLDLA/PCL blends, in the 100/0, 90/10, 80/20 and 70/30 compositions and to characterize them by SEM, DSC, GPC analyses and mechanical properties before and after degradation process phosphate buffer. 2) to accomplish the in vivo study. The in vitro results by DSC, SEM and mechanical properties until 180 days, for all the blends, presented a discreet degradation signals, and after this period, all the materials presented degraded. GPC analyses, was the most sensitive compared with others, in other words, although loss of molar mass was verified, the thermal properties are stable. The same behavior was seen in DSC analyses. The mechanical properties of blends did not present significant modifications up to 180 days of degradation, showing that with the largest addition of PCL, the blends became more elastic and less fragile. SEM analyses showed a discreet degradation of 70/30 blends in 180 days and complete degradation process for all the blends after 220 days. Based in in vitro study the 100/0 and 70/30 blends were chosen to be implanted. The results revealed that the degree of tissue organization was function of implanted time. Until the 180 days of implantation there was not differentiates relevant in vivo between pure PLDLA and the 70/30 blends. In that experiment the histological cuts revealed absence of inflammatory cells and foreign body cells reaction in the bone interface in longer periods of implants. It was predominant the ósteo-progenitors cells populating the interface, surrounded by mineralized tissue around of polymersen
dc.publisher[s.n.]pt_BR
dc.date.issued2007pt_BR
dc.identifier.citationPINTO, Marcelo Roberto. Osteointegração de blendas de PLDLA/PCL: estudo in vitro e in vivo. 2007. 92p. Dissertação (mestrado) - Universidade Estadual de Campinas, Faculdade de Engenharia Mecanica, Campinas, SP. Disponível em: <http://www.repositorio.unicamp.br/handle/REPOSIP/263821>. Acesso em: 9 ago. 2018.pt_BR
dc.description.degreelevelMestradopt_BR
dc.description.degreedisciplineMateriais e Processos de Fabricaçãopt_BR
dc.description.degreenameMestre em Engenharia Mecânicapt_BR
dc.contributor.committeepersonalnameZavaglia, Cecília Amélia de Carvalhopt_BR
dc.contributor.committeepersonalnameAlberto-Rincon, Maria do Carmopt_BR
dc.date.defense2007-10-07T00:00:00Zpt_BR
dc.date.available2018-08-10T02:09:50Z-
dc.date.accessioned2018-08-10T02:09:50Z-
dc.description.provenanceMade available in DSpace on 2018-08-10T02:09:50Z (GMT). No. of bitstreams: 1 Pinto_MarceloRoberto_M.pdf: 4314362 bytes, checksum: 9409fb084dec73adeaabc36290def760 (MD5) Previous issue date: 2007en
dc.identifier.urihttp://repositorio.unicamp.br/jspui/handle/REPOSIP/263821-
Appears in Collections:FEM - Tese e Dissertação

Files in This Item:
File SizeFormat 
Pinto_MarceloRoberto_M.pdf4.21 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.