Please use this identifier to cite or link to this item: http://repositorio.unicamp.br/jspui/handle/REPOSIP/199808
Type: Artigo de periódico
Title: Effect Of Root Canal Sealers On Bond Strength Of Fibreglass Posts Cemented With Self-adhesive Resin Cements.
Author: Cecchin, D
Farina, A P
Souza, M A
Carlini-Júnior, B
Ferraz, C C R
Abstract: This study evaluated the effects of different root canal sealers on the bond strength of a fibreglass post cemented with self-adhesive resin cements. The root canals of 50 extracted maxillary single-rooted canine teeth were prepared with the crown-down technique and randomly divided into five groups according to the sealer used: group 1: control group, gutta-percha points only (no sealer); group 2: AH Plus (resin-based sealer); group 3: self-etch Epiphany (resin-based sealer); group 4: Sealer 26 (calcium hydroxide-based sealer); and group 5: Endomethasone (zinc oxide eugenol-based sealer). The root canals were filled with gutta-percha, the cold lateral compaction technique, except for group 3 where Resilon was used. Post spaces were prepared, and fibreglass posts were cemented with the self-adhesive cement RelyX Unicem. Bonded specimens were sectioned into 1-mm-thick slabs, and a push-out test was performed in a universal machine. Failure modes were observed and classified into five types: (i) adhesive between the post and resin cement; (ii) mixed, with resin cement covering 0-50% of the post diameter; (iii) mixed, with resin cement covering 50-100% of the post surface; (iv) adhesive between resin cement and root canal; and (v) cohesive in dentine. Data of bond strength were submitted to anova and Tukey test (α = 0.05). No significant difference was detected between control group, AH Plus, Epiphany and Sealer 26 (P > 0.05). The Endomethasone group had significantly lower bond strength values than the other sealers (P < 0.05). The prevalence of mixed fractures and adhesive cement-dentine failure was verified in the eugenol-containing sealer group; in the control group, the resin-based and calcium hydroxide-based sealer groups, the predominant mode of failure was the mixed type. Endomethasone interfered negatively with the bond to root dentine; however, AH Plus, Epiphany and Sealer 26 did not interfere in the bond strength of a fibreglass post cemented with self-adhesive resin cements.
Subject: Analysis Of Variance
Calcium Hydroxide
Cuspid
Dental Bonding
Dental Stress Analysis
Dentin
Dentin-bonding Agents
Glass
Humans
Materials Testing
Post And Core Technique
Resin Cements
Root Canal Filling Materials
Root Canal Obturation
Statistics, Nonparametric
Zinc Oxide-eugenol Cement
Rights: fechado
Identifier DOI: 10.1111/j.1365-2591.2010.01831.x
Address: http://www.ncbi.nlm.nih.gov/pubmed/21219360
Date Issue: 2011
Appears in Collections:Artigos e Materiais de Revistas Científicas - Unicamp

Files in This Item:
File SizeFormat 
pmed_21219360.pdf77.19 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.